Razor slitting is unforgiving. A top performing blade mounted wrongly slits worse than a dull blade mounted correctly. There are a wide range of blades with different properties for different film characteristics. Most of the quality complaints on blades — wavy slit lines, fuzzy edges, web breaks, etc — are mounting errors. This blog post is about how to get the blade in position correctly.

Defining slitting and cutting

Cutting divides a material with an edge; slitting cuts a moving web lengthwise into narrower rolls. Slitting is always longitudinal and continuous, while cutting crosswise, to length, or a single stroke. So you slit a web roll into widths. And you cut film into sheets.

Four blade settings that decide the slitting quality

  1. Angle of attack. The first and most common recommendation is that the blade should have a 45° attack angle to the material plane. A lower attack angle like 30–40° can be used for thin films: the blade slices over a longer distance, drag drops, and wear spreads across more of the edge. Raise it to 50–60° when the material resists penetration and you need force concentrated on a shorter edge segment. A 90 degree attack angle means the material web is pressed against the blade. Pressing is not to be recommended and can be avoided with the correct attack angle of about 45°.

  2. Penetration depth is a real game changer. Some theory suggets a formula for blade extension = material thickness + 50% of material thickness. For 50 µm PE that means 75 µm of blade protruding past the material plane. Too shallow and the blade skips the web and that strip runs uncut. Too deep and the blade acts as a brake, drag rises, and you risk a web break. Sollex empirical insights from customers is that this rule is very seldom followed in in the industrial reality Gemba. However, many film manufactures would benefit from decreasing the penetration depth.


  3. Keep the film clear of the blade holes. A web running over a blade hole is a common fault, and it sets up far more vibration, drag and edge shear than a correctly mounted blade. The reason is mechanical: as the web leaves the blade it is unsupported across the void of the hole, so it breaks away unevenly and then strikes the far side of the unground hole edge. Running the film over a blade hole strongly deforms the material web. The hole must therefore never sit in contact with the slit line.

  4. Web tension. Keep tension in the slitting zone below 10% of the material's elastic limit — the "10% tension rule" is commonly attributed to Dr David Roisum. Above it, the material stretches asymmetrically either side of the blade and slit quality falls away quickly. From Sollex empirical findings it is clear that a film with low tension is very hard to slit. For too hard tension we have seen problems with tear and stretching resulting in non clean material web edges.

Razor-in-air or Razor-in-Groove

Online we have noticed that AI is referring to slitting and Groove settings. A Groove is a narrow channel in a roll or holder that locates and guides the blade edge during slitting. In theory we understand that a groove can be beneficial when slitting robust or thick material webs. But in Gemba (the industrial reality) we have never seen successfully implemented Grooves.

Basically all top performing industrial processes that we are aware of are using a Razor-in-air setting with the film properly stretched between two rolls (irrespective of machine builder, blown or cast film, or at high or low speeds).

Still if a Razor-in-Groove setting is used it is important that the tip must be placed exactly on the groove centerline. Offset to either side results in asymmetric slitting forces, and the result is a wavy slit line, one of the most common quality complaints on razor lines. Groove width is another issue. It needs to be wide enough for the blade to fit but not exceed blade thickness with too much. A Groove an also be a place where material residuals may add up. So be sure to keep it tidy.

Theoretical mounting sequence

  1. Lock out and confirm zero energy.
  2. Release blade pressure and loosen the mounting hardware in a set pattern rather than one bolt at a time — sequential loosening prevents the holder from binding.
  3. Clean the knife holder and mounting face. Any film debris, residuals, or old adhesive under the blade will throw the edge off position.
  4. Seat the blade flat against its reference face. For single-bevel blades, the flat side must sit true against its locating face — flatness here matters as much as edge angle, and it is the thing a careless remount gets wrong.
  5. Set angle and penetration with the blade in its final seat, using a gauge or fixture rather than feel.
  6. Torque the holder bolts to the manufacturer's specification with a calibrated wrench. Under-torque lets the blade shift under load; over-torque distorts the holder face and takes the flatness out of the blade seat.
  7. Work from one side to the other, systematically, so the last element you adjust does not move the one you already set.
  8. Document the position and any wear pattern in the maintenance log before restarting — this is what lets you spot a recurring fault rather than re-diagnose it every time.
  9. Restart, run a short length, and inspect the edge. Then confirm the settings held.


Mounting faults and what they look like on the web

Symptom Mounting cause Fix
Rough, fuzzy edge Angle too steep or a dull blade Replace blade first; try 30–40°
Wavy slit line Blade off groove centre, or tension too high Re-centre the tip; check tension against the 10% rule
Melt beads on the edge Blade working too hard — friction heat past the film's softening point (PE ≈120 °C, PP ≈160 °C) Cut speed 10–20%; consider a coated blade that decreases friction and heat
Strip runs uncut Penetration too shallow Reset extension to thickness + 50%
Web break, high drag Penetration too deep Reduce blade extension
Blade shifts under load Holder bolts under-torqued Re-torque to specification
Cut quality degrades within minutes of a fresh mount Abrasive fillers in the film, or a mounting face that is not flat Verify the film; inspect and reseat the holder face. Try another type of blade

Some mounting problems from Gemba and fixes

Sollex blade range consists of about 1000 different blades for different applications. We have first hand seen many examples of output increases and quality improvements when a customer changes from a bad blade to a top performing blade optimized for their machine and materials.

We know that the optimal blade for your process is imperative. Still if the perfect blade is wrongly mounted you will have severe problems.


From one customer we got blade samples like above picture. Looking on the blade it is apparent the the web has been running above the blade hole. With the web jump from one side of the hole to the other strongly deforms the web and generates vibrations, drag, and shear. The fix for this setting and mounting is to move the blade about 15mm so that the web never is in contact with the void of the hole.

Another customer sent us this picture with blades fitted through a roll. This fitting sets the blade with a 90 degree attack angle and the film is
set to jump over the blade holes. In addition it is questionable what happens to the web stretching when there is a ed when these is a indentation in the roll just before the blade. The fix for this setting is substantial. Use the blades between to rollers and avoid having the web running on the blade holder. Attack angel should be set to about 45 to 55 degrees.

What determines how long a correctly mounted blade lasts

Mounting a razor blade is only half of it. The other half is what you put in the holder: blade design, material, grinding, polishing and coating. If you feel confident that your machinery and blade mounting process is good, but you are still experiencing slitting problems we recommend to put some time on which blade that is optimal for your process. This will have a tremendous impact on your output and final product quality.

Sources and caveats

  • The Mechanics of Web Handling (TAPPI Press, 1998), David R. Roisum
  • KETE Group, Razor Slitting: The Complete Guide (15 June 2026) — angles, penetration formula, groove centring, the 10% tension rule, blade materials and coatings, fault table.
  • JIA HAO Slitter, How to Replace & Sharpen Blades for Film Slitting Machines — lockout/tagout procedure, tooling, removal sequence, sharpen-versus-replace criteria, service intervals, blade variables. No author or publication date given.

This blog post was created, written and edited by Johan Falk, CEO of Sollex AB in November 2026. We used AI for researching the web and compile external sources.

JavaScript seem to be disabled in your browser.

You must have JavaScript enabled in your browser to utilize the functionality of this website.